Galvanic Corrosion: Galvanic Series Chart and How to Prevent It

Galvanic corrosion: galvanic series chart in seawater and how to prevent dissimilar metal corrosion with stainless steel

Galvanic Corrosion: Galvanic Series Chart and How to Prevent It

Will Lee - Account Manager, European Market at TeCarve
Will Lee
November 20, 2026
15 Min Read

Galvanic corrosion is the faster corrosion of one metal caused by electrical contact with a more noble metal while both are wet with the same electrolyte. The less noble metal (the anode) corrodes more than it would alone, and the more noble one (the cathode) corrodes less. A galvanic series ranks metals by their corrosion potential in a given environment; in seawater, passive stainless steel sits near the noble end, close to titanium and nickel alloys, while carbon steel, aluminum and zinc sit at the active end. It is prevented by choosing metals close together in the series, insulating the joint, keeping water out of it, or keeping the anode large and the cathode small.

What is galvanic corrosion?

Three things have to be present at the same time: two different metals (or a metal and a conductor such as graphite), an electrical path between them, and an electrolyte, which can be seawater, cooling water, condensate, wet soil or even a film of salty moisture. Remove any one of the three and the galvanic effect stops. MIL-STD-889C calls the metals “dissimilar” when, in contact in a conductive solution, they can generate an electric current.

The current flows from the more active metal into the electrolyte and back through the contact to the more noble metal. Metal leaves the anode as ions, so the damage concentrates on the anode, usually close to the joint where the current path is shortest. The cathode is partly protected at the same time, which is why a stainless steel bolt in a steel plate can look perfect while the plate around it is eaten away.

Galvanic series chart (seawater)

The table below follows Figure 1 of ASTM G82, a galvanic series measured in flowing seawater (2.4 to 4.0 m/s, 5 to 30 °C, 5 to 15 days) against a saturated calomel electrode. The potential ranges were read from the figure and are approximate. Stainless steels and some nickel alloys appear twice, because they can be either passive or active:

Metal or alloy (noble at the top)Corrosion potential, V vs SCE (approx.)Note
Graphite+0.20 to +0.31
Platinum+0.19 to +0.25
Ni-Cr-Mo alloy C (C-276 family)−0.03 to +0.09
Titanium−0.05 to +0.06
Alloy 825 (Ni-Fe-Cr)−0.02 to +0.05
Alloy 20 stainless (cast and wrought)−0.04 to +0.05
Stainless steel 316, 317 – passive−0.10 to 0.00Normal state in aerated, flowing water
Ni-Cu alloy 400, K-500−0.15 to −0.02
Stainless steel 302, 304, 321, 347 – passive−0.09 to −0.04
Nickel 200−0.20 to −0.09
Ni-Cr alloy 600 – passive−0.18 to −0.14
Nickel-aluminum bronze−0.21 to −0.15
70-30 copper-nickel−0.23 to −0.17
Stainless steel 430 – passive−0.27 to −0.20
90-10 copper-nickel−0.29 to −0.22
Stainless steel 410, 416 – passive−0.35 to −0.26
Admiralty brass, aluminum brass−0.35 to −0.27
Pb-Sn solder (50/50)−0.35 to −0.28
Copper−0.38 to −0.31
Naval, yellow and red brass−0.40 to −0.30
Aluminum bronze−0.42 to −0.32
Stainless steel 316, 317 – active−0.46 to −0.36In crevices, under deposits or in stagnant, low-oxygen water
Stainless steel 302, 304, 321, 347 – active−0.57 to −0.47
Austenitic nickel cast iron−0.56 to −0.44
Low alloy steel−0.62 to −0.57
Mild (carbon) steel, cast iron−0.72 to −0.60
Cadmium−0.74 to −0.69
Aluminum alloys−1.01 to −0.77
Zinc−1.04 to −0.99
Magnesium−1.63 to −1.60

Read from ASTM G82-98 (2014), Fig. 1, which the guide notes was redrawn from an earlier published series; values are corrosion potentials, not standard electrode potentials, and apply to seawater only.

Why stainless steel appears twice

Stainless steel stays passive while its chromium oxide film is intact, which needs oxygen at the surface. In aerated, moving seawater that is the normal state, and the steel behaves almost like titanium. Inside a crevice, under a gasket, beneath fouling or in stagnant water, oxygen is used up and the film can break down; the steel then becomes active and its potential drops by roughly 0.3 to 0.5 V. That has two consequences. A passive stainless part is a strong cathode for carbon steel, aluminum or zinc it touches. And a small active area on a stainless part, such as a crevice under a flange gasket, can itself become the anode of a cell whose cathode is the surrounding passive steel.

Stainless steel in contact with other metals

For piping, the common couples are stainless pipe on carbon steel supports, stainless connected to copper or brass in water systems, and stainless fasteners in aluminum or galvanized structures. The differences below are calculated from the ranges in the chart; a larger difference means a larger driving force, but, as G82 points out, not always a proportionally larger attack:

Couple in seawaterPotential difference (from G82 Fig. 1)Metal that corrodes fasterRisk and action
316 (passive) + carbon steelabout 0.50 to 0.72 VCarbon steelHigh: insulate, or coat both sides of the joint
304 (passive) + aluminum alloyabout 0.68 to 0.97 VAluminumVery high: insulate; never use aluminum fasteners on stainless
316 (passive) + galvanized steel (zinc)about 0.89 to 1.04 VZinc coatingVery high: the zinc is consumed locally at the joint
316 (passive) + copperabout 0.21 to 0.38 VCopperModerate: lower risk in fresh water than in seawater; insulate in seawater or where the copper part is small
316 (passive) + 90-10 copper-nickelabout 0.12 to 0.29 VCopper-nickelModerate
316 (passive) + C-276 family (Ni-Cr-Mo alloy C)overlapping rangesLittle differenceLow: close together on the series
316 (passive) + titaniumoverlapping rangesLittle differenceLow
316 passive + 316 active (same steel)about 0.26 to 0.46 VActive area (crevice)The same alloy can couple with itself: a crevice becomes the anode

How to prevent galvanic corrosion

  1. Choose metals close together in the series. MIL-STD-889C (5.1.1) puts it simply: the closer two metals are in the series, the more compatible they are. Joining 316L to C-276-type nickel alloys or titanium raises little concern; joining it to carbon steel or aluminum does.
  2. Break the electrical path. Isolating flange kits (non-conductive gaskets, bolt sleeves and washers), dielectric unions or insulating spool pieces stop the current. Check that the path is not completed elsewhere, through a pipe support, an earthing strap or a common steel frame. MIL-STD-889C (5.1.2) also lists an inert, non-absorbing barrier or sealant between faying surfaces.
  3. Keep the electrolyte out. Sealing the joint so it stays dry, or painting, prevents the cell from forming. If only one metal can be coated, coat the cathode (the stainless or copper side): a scratch in paint on the anode leaves a tiny anode facing a huge cathode, which concentrates the attack.
  4. Get the area ratio right. A small anode coupled to a large cathode corrodes fast; the reverse is usually tolerable. MIL-STD-889C (5.1.3) requires small anodic areas to be avoided and fasteners to be of the same or a more noble metal. Stainless bolts in an aluminum or steel structure are therefore acceptable far more often than steel or aluminum bolts in a stainless one.
  5. Use a sacrificial or intermediate material where needed. MIL-STD-889C allows a sacrificial coating on the cathode with a potential close to the anode, or an interposed material compatible with both metals (5.1.2, 5.1.4).
  6. Design out crevices. Smooth, fully drained, well-fitted joints keep stainless steel passive and avoid the active-passive cell on the same part; higher-PREN grades resist the breakdown longer (see the PREN calculator).

Limits of the galvanic series

  • It applies to one environment. G82 (5.2) warns that a series measured in flowing ambient-temperature seawater should not be used for fresh water or heated seawater. Fresh water conducts far less than seawater, so the same couple usually causes less attack there, but it has its own series.
  • Potentials move. They change with time, temperature and flow, and positions can even reverse (G82 5.3).
  • It predicts direction, not rate. The series tells which metal will suffer, not how fast (G82 5.5). Area ratio, electrolyte conductivity, the distance between the metals, deposits and polarization all change the rate (G82 5.7). For a rate, galvanic corrosion tests are needed (ASTM G71).
  • It is not the electromotive (EMF) series. Standard electrode potentials of pure elements are a different list and should not be used to predict galvanic corrosion (G82 5.1).

For how stainless steel compares with the metals it is most often joined to, see carbon steel vs stainless steel and stainless steel vs galvanized pipe; for why stainless steel can still rust, see does stainless steel rust?.

TeCarve is the exclusive factory-direct export channel for two dedicated manufacturing plants in Foshan (welded & decorative tubing) and Wenzhou (seamless & precision tubing). When stainless pipe or tube will be connected to carbon steel, copper alloy or aluminum equipment, say so in the enquiry so that grade and connection details can be discussed before quotation.

Sources: ASTM G82-98 (Reapproved 2014), Standard Guide for Development and Use of a Galvanic Series for Predicting Galvanic Corrosion Performance (sections 3–5, Figs. 1 and 2); MIL-STD-889C, Dissimilar Metals (22 August 2016), sections 3 and 5.

Written by Will Lee, Account Manager (Europe), TeCarve · Reviewed against ASTM / EN / ISO source documents · How we write and review our technical guides →
Will Lee - Account Manager, European Market at TeCarve

Author: Will Lee

Will Lee is TeCarve's Account Manager for Europe and the author of TeCarve's technical guides on stainless steel pipe and tube. His article on ASTM A312, A213 and A249 tubing was published in Stainless Steel World (October 2026). He reviews buyer specifications and drawings against ASTM, EN and DIN standards, advises on grade, tolerance and testing requirements, and checks the mill test certificates issued by the producing plants before European shipments.